Выделение титана из титаномагнетитовой руды В. В. Орлов, Р. О. Медведев, И. В. Амеличкин

By: Орлов, Владислав ВикторовичContributor(s): Медведев, Родион Олегович | Амеличкин, Иван ВячеславовичMaterial type: ArticleArticleOther title: Extraction of titanium from titanomagnettis [Parallel title]Subject(s): переработка руды | выщелачивание | дробление | рентгенофазовый анализ | экспериментальные данные | титаномагнетитовые руды | диоксид титанаGenre/Form: статьи в сборниках Online resources: Click here to access online In: Перспективы развития фундаментальных наук. Т. 2 : сборник научных трудов XV Международной конференции студентов, аспирантов и молодых ученых, 24–27 апреля 2018 г Т. 2 : Химия. С. 234-236Abstract: In this paper, we study the possibility of obtaining iron and titanium-vanadium concentrates with highest contents of iron and titanium, respectively, through hydrometallurgical processing of the titanomagnetite ores of the Chineisk deposit. Ammonium fluoride concentration was varied from 0.08 mol/L to 4.2 mol/L with the other fixed parameters. It was shown that optimum ammonium fluoride concentration for leaching the ore is 0.42 mol/L. The acidity of solution was changed by adding of hydrofluoric acid with varied concentration (from 0.86 mol/L to 4.07 mol/L) to ammonium fluoride solution with fixed concentration of 0.42 mol/L. The best results (degree of titanium extraction = 63.7%) were obtained when using a solution of hydrofluoric acid with concentration 4.07 mol/L.
Tags from this library: No tags from this library for this title. Log in to add tags.
No physical items for this record

Библиогр.: 5 назв.

In this paper, we study the possibility of obtaining iron and titanium-vanadium concentrates with highest contents of iron and titanium, respectively, through hydrometallurgical processing of the titanomagnetite ores of the Chineisk deposit. Ammonium fluoride concentration was varied from 0.08 mol/L to 4.2 mol/L with the other fixed parameters. It was shown that optimum ammonium fluoride concentration for leaching the ore is
0.42 mol/L. The acidity of solution was changed by adding of hydrofluoric acid with varied concentration (from 0.86 mol/L to 4.07 mol/L) to ammonium fluoride solution with fixed concentration of 0.42 mol/L. The best results (degree of titanium extraction = 63.7%) were obtained when using a solution of hydrofluoric acid with concentration 4.07 mol/L.