Влияние напряжения и длительности микродугового оксидирования на физические характеристики стронций- и кремний-содержащих биопокрытий Я. О. Иващенко, Е. Г. Комарова, Е. А. Казанцева

By: Иващенко, Яна ОлеговнаContributor(s): Комарова, Екатерина Геннадьевна | Казанцева, Екатерина АлександровнаMaterial type: ArticleArticleOther title: Influence of micro arc oxidation voltage and duration on physical characteristics of strontium- and silicon-containing biocoatings [Parallel title]Subject(s): биопокрытия | кальций-фосфатные покрытия | стронций | кремний | микродуговое оксидирование | формирование покрытийGenre/Form: статьи в сборниках Online resources: Click here to access online In: Перспективы развития фундаментальных наук. Т. 1 : сборник научных трудов XV Международной конференции студентов, аспирантов и молодых ученых, 24-27 апреля 2018 г Т. 1 : Физика. С. 144-146Abstract: The investigations ofphysical characteristics of Sr- and Si-containing calcium phosphate coatings formed by micro arc oxidation method under different pulsed voltage 200-370 V for various time were performed. The coating thickness grow by exponential law with increasing of the process duration, but the coating roughness and apparent density do not vary, in this case. The increase in the process voltage leads to the linear increase in the coating thickness and roughness from 55 to 150 pm andfrom 3.2 to 8.8 pm, respectively.
Tags from this library: No tags from this library for this title. Log in to add tags.
No physical items for this record

Библиогр.: 3 назв.

The investigations ofphysical characteristics of Sr- and Si-containing calcium phosphate coatings formed by micro arc oxidation method under different pulsed voltage 200-370 V for various time were performed. The coating thickness grow by exponential law with increasing of the process duration, but the coating roughness and apparent density do not vary, in this case. The increase in the process voltage leads to the linear increase in the coating thickness and roughness from 55 to 150 pm andfrom 3.2 to 8.8 pm, respectively.

There are no comments on this title.

to post a comment.
Share